Acid Resistant Mortar in Kenya, Tanzania, Uganda, Rwanda
Acid Resistant Mortar
Bituminous Primer :
It is bituminous air curing ready mixed acid and alkali resistant primer.
Mastic :
It is acid and alkali resistant mastic used as a protective impervious membrane suitable for concrete, brickwork, steel, etc.
Furan Resin Mortar :
It is widely used for acid resistant bricks and tiles lining work as bedding and joining mortar for tanks, floors, drain, foundation, chemical reaction vessel, neutralization pit etc.
Properties :
– Working time at 30’C : 20 Minutes(min)
– Density of cured mortar : 1.8 gm/cc
– Bond Strength : 10 Kg.cm2
– Compressive Strength : 350 Kg.cm2
– Flectual Strength : 75 Kg.cm2
Phenolic Resin Mortar :
It is widely used for acid resistant bricks and tiles lining work as bedding and joining mortar for tanks, floors, drain, foundation, chemical reaction vessel, neutralization pit etc.
Properties :
– Working time at 30’C : 20 Minutes(min)
– Density of cured mortar : 1.8 gm/cc
– Bond Strength : 10 Kg.cm2
– Compressive Strength : 350 Kg.cm2
– Flectual Strength : 75 Kg.cm2
– Water Absorption : 1%
CNSL Resin Mortar :
It is widely used for lining of acid resistant bricks as bedding and joining mortar It can also be used for jointing chemical resistant stoneware pipes and ETP Plants.
It is suitable where excellent resistance properties and heavy impacts subjected to the surface of floors and tank is required. It can also be applied as monolithic lining for construction pf dilute acids storage tanks.
Potassium Silicate Acid Resistant Mortar :
It is widely used for acid and alkali resistant bricks/tiles as bedding and joining mortar for tanks, floors, drain, foundation etc. It has a temperature resistance upto 1000˚C.
Properties :
– Working time at 30˚C : 20 Minutes(min)
– Density of cured mortar : 2.0 gm/cc
– Bond Strength : 5 Kg.cm2
– Compressive Strength : 150 Kg.cm2
– Flexural Strength : 40 Kg.cm2
– Toluene Absorption : 18%(max)
Sodium Silicate Acid Resistant Mortar :
It is widely used for acid resistant bricks/tiles as bedding and joining mortar for tanks, floors, drain, foundation etc. It is useful in pH range of 0-6 or in concetration above 93%. It has a temperature resistance upto 1000˚C
Properties :
– Working time at 30˚C : 15 Minutes(min)
– Density of cured mortar : 2.0 gm/cc
– Bond Strength : 5 Kg.cm2
– Compressive Strength : 100 Kg.cm2
– Flexural Strength : 40 Kg.cm2
– Toluene Absorption : 18%(max)
Sulpher Based Acid Resistant Mortar :
It is a sulpher based mortar containing plasticizer and filler. The melt mortar is extremely fluid and pours quite easily. It is resistant to non-oxidizing acids and neutral salts. It has a temperature resistance upto 90˚C(max).
Properties :
– Density of cured mortar : 2.1-2.2 gm/cc
– Bond Strength : 10 Kg.cm2
– Compressive Strength : 280 Kg.cm2
– Flexural Strength : 70 Kg.cm2
– Water Absorption : 1%